Can I color finished carbon fiber parts?


Author
Message
Leviatano55
Leviatano55
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 3, Visits: 51
polaraligned (15/05/2017)
I would be interested to see what a part looks like with a tinted clear coat on top. 
Ill post pictures when I finish 
But until then here are some Pagani's finished in purple blue and green carbon to give you an idea of tinted clear coats. These cars are actually my inspiration for putting some green carbon accents on my green boxster. 

https://scontent.cdninstagram.com/t51.2885-15/e35/14701339_212054012560421_7154713833443950592_n.jpg?ig_cache_key=MTM2ODE4NjA5MzU4MDg2NjA3MQ%3D%3D.2
https://i.kinja-img.com/gawker-media/image/upload/s--oR5lwv0t--/c_fill,fl_progressive,g_center,h_450,q_80,w_800/nyx5xe0rvsdtywaqny4j.jpg
http://2.bp.blogspot.com/-QHHBzPSzhyg/U02TI8yzvoI/AAAAAAAAAbU/v3nPaVcCpe8/s1600/Scopione-USA-Pagani-Sports-Car-On-Fire-in-Geneva-2014-Blue-Carbon-Fiber-Gone-Wild+%25283%2529.jpg
Edited 8 Years Ago by Leviatano55
polaraligned
polaraligned
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 13, Visits: 284
I would be interested to see what a part looks like with a tinted clear coat on top. 
Leviatano55
Leviatano55
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 3, Visits: 51
Interloper393 (14/05/2017)
Candy paints are great over carbon pieces,  then clear coat them
I agree, I think it vastly improves the look of carbon fiber. 
Hanaldo (13/05/2017)
Absolutely, no problem. 
Thanks!
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Candy paints are great over carbon pieces,  then clear coat them
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Absolutely, no problem. 
Leviatano55
Leviatano55
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 3, Visits: 51
I just bought my first sports car (Porsche Boxster) and I want to give it a touch of carbon fiber on the exterior. I am planning on buying two exposed carbon fiber mirrors. Would I be able to add two extra clear coats (one tinted) to give it a colored carbon look, or can I not paint carbon once it is fully finished? 
thanks

Edited 8 Years Ago by Leviatano55