Marking out and stopping fraying


Author
Message
rmaddock
rmaddock
Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)
Group: Forum Members
Posts: 17, Visits: 1.5K
Good morning all you composite people!

I've been trying to use masking tape on my lovely expensive fabric (210g carbon/kevlar twill) both to mark it out for cutting (ie drawing on the tape, not the fabric) and to prevent the edges thus formed from fraying.

I've tried el-cheapo masking tape from a certain major UK DIY retailer; it sticks too well and I makes a mess as I peel it off.

I've tried both orange and green "frog" tape (I had both colours lying about) and that certainly doesn't stick too much. In fact it hardy sticks at all and lifts off whilst I'm trying to cut along my lines.

What else do people use/do to mark fabrics and protect the edges please?

Thanks,
Robert.
Reply
WR Composites
WR Composites
Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)
Group: Forum Members
Posts: 9, Visits: 158
A light coat of Fusion fix gp or cheap hair spray along the cut line works fine.