Good morning all you composite people!

I've been trying to use masking tape on my lovely expensive fabric (210g carbon/kevlar twill) both to mark it out for cutting (ie drawing on the tape, not the fabric) and to prevent the edges thus formed from fraying.

I've tried el-cheapo masking tape from a certain major UK DIY retailer; it sticks too well and I makes a mess as I peel it off.

I've tried both orange and green "frog" tape (I had both colours lying about) and that certainly doesn't stick too much. In fact it hardy sticks at all and lifts off whilst I'm trying to cut along my lines.

What else do people use/do to mark fabrics and protect the edges please?

Thanks,
Robert.
Reply
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
They seem to stay sharp for quite a long while. I've been using my current blade nearly every day for the last couple of months and it'll still cut through 650g fabric without too much drama

I've placed large self-healing cutting mats on my table, so the cutter makes quick work of simple straight cuts and it's quick and neat on curved cuts as well.  