Mold from ABS plastic part
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Dan22h
Dan22h
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 15,
Visits: 197
I have an abs plastic wheel arch liner for my car that I would like to take a mold from. I've read online that styrene based resins react with the ABS, is there any way around this such as suitable release agents? The part is not visible so surface finish isn't an issue.
Reply
Like
3
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
PVA release agent mate. Or packing tape.
Reply
Like
2
Fasta
Fasta
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Are you sure it's ABS ?
The majority of modern
plastic car bumper
system fascias are made of thermoplastic olefins (TPOs), polycarbonates, polyesters, polypropylene, polyurethanes, polyamides, or blends of these with, for instance, glass fibers, for strength and structural rigidity.
Fastacraft Facebook page
Reply
Like
2
Dan22h
Dan22h
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 15,
Visits: 197
It's an inner wheel arch liner for a lotus exige, there's a paper sticker on the back with recycling logo ♻ >ABS<
Looks like this
Edited
9 Years Ago by
Dan22h
Reply
Like
3
Fasta
Fasta
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Do your own small test on the back of the part.
Some wax, some PVA and just a tiny bit of your preferred tooling gelcoat to see if it reacts.
Fastacraft Facebook page
Reply
Like
3
Dan22h
Dan22h
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 15,
Visits: 197
OK, thanks for the replies.
Reply
Like
3
FLD
FLD
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
They are abs. I'd go with the pva. Dust a light coat on with a spay gun and let it dry. Keep applying dust coats until you have an even blue coat then put down a few full film coats letting it dry between each coat. I then do a single coat of wax and grp just falls off!
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search