I want to make a 2-part mould roughly covering 3.5sqmtrs but the overall cost is quite large.

Would it be possible to use a cheaper alternative to the Uni-mould Tooling resin (which appears to be the most expensive part) such as a cheap Polyester resin to bond all the layers of chopped strand mat? Or is there another cheaper alternative to the uni-mould system that would give adequate results?

I don't intend on pulling hundreds of releases, at most I would say 5 in total?
Replies
Junior
Junior
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 73, Visits: 473
GP resin is fine mate, it is the cheaper alternative 


What about the gelcoat/coupling coat?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Junior (21/04/2017)
GP resin is fine mate, it is the cheaper alternative 


What about the gelcoat/coupling coat?


GP resin will bond ok to vinyl ester gelcoat, so you can use that. The reason the coupling coat is there is that mineral filled resins tend to trap voids behind the gelcoat, so you can't use the Unimould tooling resin directly behind the gelcoat. The coupling coat is also a vinyl ester laminating resin so it will shrink less and print less. 

You can also use a regular vinyl ester laminating resin rather than a coupling coat. Coupling coats are considered a 'premium' laminating resin, so they are better but a bit more expensive. A regular vinyl ester would be better than a regular polyester if you can stretch the budget. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Junior - 8 Years Ago
FLD - 8 Years Ago
Junior - 8 Years Ago
Hanaldo - 8 Years Ago
Junior - 8 Years Ago
Hanaldo - 8 Years Ago
oekmont - 8 Years Ago
Junior - 8 Years Ago
Hanaldo - 8 Years Ago
oekmont - 8 Years Ago
Junior - 8 Years Ago
Junior - 8 Years Ago
Dravis - 8 Years Ago
Junior - 8 Years Ago
Hanaldo - 8 Years Ago
Junior - 8 Years Ago
Hanaldo - 8 Years Ago
oekmont - 8 Years Ago
Junior - 8 Years Ago
oekmont - 8 Years Ago
Junior - 8 Years Ago
FLD - 8 Years Ago
Junior - 8 Years Ago
FLD - 8 Years Ago
Hanaldo - 8 Years Ago
Junior - 8 Years Ago
oekmont - 8 Years Ago
Hanaldo - 8 Years Ago
FLD - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search