Vinyl as a release layer?


Author
Message
Junior
Junior
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 73, Visits: 473
Does anyone know if tooling gelcoat sticks to vinyl?

I just wondered if vinyl could be applied to a plug as a temporary smooth release layer before applying a tooling gelcoat to make a mould rather than prepping it with release agents/wax?
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Try it lol
Junior
Junior
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 73, Visits: 473
Unfortunately I don't have any tooling gelcoat yet.

Would epoxy laminating resin have similar results as I have some of that I could try against vinyl?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Negative, vinyl is no good unless you're using PVA. 
Junior
Junior
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 73, Visits: 473
Negative, vinyl is no good unless you're using PVA. 


Thanks Hanaldo!