By Junior - 3/28/2017 12:26:08 PM

Does anyone know if tooling gelcoat sticks to vinyl?

I just wondered if vinyl could be applied to a plug as a temporary smooth release layer before applying a tooling gelcoat to make a mould rather than prepping it with release agents/wax?
By Junior - 4/1/2017 8:14:21 AM

Negative, vinyl is no good unless you're using PVA. 


Thanks Hanaldo!