Hi all!


I’ve recently discovered the world of composites and have been fascinated with the whole subject and intrigued with what can be produced.


I am a very keen kayaker and have a burning desire to build a composite version of my current plastic surf boat, a Fluid Element which weighs around 15kgs and measures 202cm x 64cm (widest part).



I have tried paddling some other boats which are produced in carbon/kevlar, but due to their design I just haven’t got on with them aswell as my current boat. 

My boat was produced in carbon/kevlar in a limited amount (around 30), but these are very rare to come by and as you can imagine, fetch a large amount of money as they retailed at £1395 new. I am therefore planning a long-term project to build myself a composite version but have come across the usual problems that most people encounter such as which combination of materials to use.


I will be on a tight budget with not much room for error, so I need to keep costs down by using cheaper materials/resins if possible. I plan to take a mould of my current boat in either two or three parts, then create the boat using wet-lay and vacuum bagging.


My initial thoughts are one of the following four lay-ups with Polyester/Vinylester resin with a target weight under 9kgs:


(From Outside the boat to Inside the boat)


Outer layer of 300g Black Diolen 2/2 twill

1x 300g plain Diolen 2/2 twill

3mm foam core

1x 300g plain Diolen 2/2 twill

1x 300g Black Diolen 2/2 twill


or (if the Diolen only lay-up is not stiff enough)…


Outer layer of 300g Black Diolen 2/2 twill

1x 300g S-Glass 2/2 twill

3mm foam core

1x 300g S-Glass 2/2 twill

1x 300g Black Diolen 2/2 twill


or (if the lay-up needs to be stronger still)…


Outer layer of 300g Kevlar 2/2 twill

1x 300g Carbon 2/2 Twill

3mm foam core

1x 300g Carbon 2/2 twill


Or (if my budget will stretch to it)…


2 x 228g Carbon/Kevlar Aramid

3mm Foam Core

2x 228g Carbon/Kevlar Aramid


My question is, firstly will the lay-ups be strong enough for white water use in the sea (waves) with the odd scrape and knock from pebbly beaches? It will no doubt take more of a beating than a longer sea kayak as it’s more of a play boat style kayak. And secondly, which lay-up will be stronger? I could possible use a mixture of the lay-ups with a stronger/more expensive one making up the base of the kayak, and a cheaper one making up the top half of the kayak?


I have chosen to put either the Diolen or Kevlar on the outside layer to give better abrasion resistance and to protect the Carbon/S-Glass, however I have found some conflicting information online that suggests the Kevlar/Diolen should be on the inner layer?? Being that Kevlar/Diolen can take more damage before splitting, I would have thought if it were on the inner layer, the carbon would crack on the outside before the Kevlar/Diolen, whereas on the outside it would keep the cracked carbon beneath the layer of Kevlar/Diolen protecting the boat from splitting?


Pages where I have gathered inspiration has come from:


Kevlar Playboat:

http://shanesliquidlogic.blogspot.co.uk/2011/12/composite-playboat-prototype-1.html


Carbon Zet Playboat:

https://www.youtube.com/watch?v=IA9vkauvxGY


Carbon Vadja Playboat:

http://vajdafreestyle.com/en/Kayaks/Beast/Beast-series/


Lots more questions to follow no doubt, but any help/suggestions would be fantastic!


Cheers,

Junior.


Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I would do this as an infusion, with a 2 or 3 mm Soric core and the biaxial glass   Stack:   Carbon/kevlar - Glass - Soric - Glass - Carbon/kevlar

I did a set of motorbike fairing panels like this, except with 300 gsm biaxial Carbon instead of the biaxial glass, and they came out way stiffer and stronger than needed, and too heavy as well-
I ended up doing without the core -- and with only one layer of Biaxial Carbon- -

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 8 Years Ago by Dravis
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Junior - 8 Years Ago
RedLegsGear - 8 Years Ago
Junior - 8 Years Ago
Junior - 8 Years Ago
RedLegsGear - 8 Years Ago
FLD - 8 Years Ago
Junior - 8 Years Ago
FLD - 8 Years Ago
Junior - 8 Years Ago
Junior - 8 Years Ago
Warren (Staff) - 8 Years Ago
Junior - 8 Years Ago
Warren (Staff) - 8 Years Ago
Junior - 8 Years Ago
FLD - 8 Years Ago
Junior - 8 Years Ago
FLD - 8 Years Ago
Junior - 8 Years Ago
Junior - 8 Years Ago
Dravis - 8 Years Ago
Junior - 8 Years Ago
Dravis - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search