EL2 Laminating epoxy with slow hardener is not curing


Author
Message
Drew
Drew
Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)
Group: Forum Members
Posts: 5, Visits: 42
Hi, I have used EL2 resin with slow hardener to coat the inside of a moulding with the intention of sanding and polishing it to give it a nice finish on both sides, its been 4 days now and the surface is still not hard enough to sand.

When I have done this before with the fast hardener it is good to sand after 24 hours or so,

Is it just a matter of leaving it for longer, or have I messed up somehow?.

Any Ideas,




Drew.
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi Drew,

You can seal the surface with GlassCast rather than need 2 separate resin systems.  The GlassCast has better UV resistance than the EL2 overall.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search