Hi, I have used EL2 resin with slow hardener to coat the inside of a moulding with the intention of sanding and polishing it to give it a nice finish on both sides, its been 4 days now and the surface is still not hard enough to sand.

When I have done this before with the fast hardener it is good to sand after 24 hours or so,

Is it just a matter of leaving it for longer, or have I messed up somehow?.

Any Ideas,




Drew.
Reply
JDUB
JDUB
Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)
Group: Forum Members
Posts: 10, Visits: 26
I think I will try wetting the hardener cup before I weigh out. Should retain the same amount. Would weigh in 1, but it starts to gel too fast.
Edited 8 Years Ago by JDUB
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search