Hi,
just wondering how much area will 5kg of Epoxy Mould Making Putty will cover.
According to your "Epoxy Mould Making Starter Kit" manual 750g will cover about 40cm x 40cm, so 5kg would cover about 2,66 sqm?
Thanks

Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi,

Well, actually I think to be sufficiently strong I would recommend the small kit be used for a mould no larger than 30cm x 30cm (it does depend on the shape but 40cm x 40cm would be a bit too thin I think). I've updated the product instructions and product pages accordingly.

As for your calculation on the larger kit; I think you've worked that out wrong. Remember you're talking about area so you can't just multiply both measurements to arrive at the new area; area is a square function:

750g is good for 0.3m x 0.3m = 0.09sqm
5kgs is (5/0.75) 6.6 times more material so would be good for 6.6 x 0.15sqm = 0.6sqm. In measurements: sqrt (0.6sqm)=0.77m x 0.77m

I hope this helps.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 14 Years Ago by Matt (Staff)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search