Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Skinning my work top
Skinning my work top
Post Reply
Like
3
Skinning my work top
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Richb007
Richb007
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 29
Hi
A total novice here.
Im wnt to cover my kitchen work tops in red highlighted crbon fibre
.
Iv been playing with the idea for sometime and have read and watched lots of stuff, i think its possible for me to do without cocking it up.
Any advice on resin, techniques equipmennt and where to get appreciated.
R
Reply
Like
3
Reply
Richb007
Richb007
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 29
Yes i thought you'd say heat but there seems to be heat resistant resin that is used in engine parts and i cant see it being much more vulnerable as timber with water or even granite with oil. Both are terrible kitchen work surfce materials in my view, they just look nice.
It seems you work in the industry, if i send the measurements can you quote for the materials???
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Skinning my work top
Richb007
-
8 Years Ago
HI, The technique for skinning on a worktop would be exactly the same as any other item, albeit...
Warren (Staff)
-
8 Years Ago
Yes i thought you'd say heat but there seems to be heat resistant resin that is used in engine parts...
Richb007
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search