Reduction of weight in the manufacture of a kayak


Author
Message
Almand
Almand
Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)
Group: Forum Members
Posts: 19, Visits: 108

Theme:

Reduction of weight in the manufacture of a kayak with the use of the sandwich material Easy Cell 75 Closed Cell Foam PVC, 3 mm thickness.

 

We have previously used Soric 3mm in a construction of a kayak with one layer of carbon fiber and one layer of Kevlar, then sorric as sandwich and finally a layer of carbon fiber, all produced in a single resin vacuum process.  A strong construction, but a little too heavy.

 

To reduce the weight we have now used Easy Cell 75 Closed Cell PVC Foam, 3mm thickness as sandwich.

In the design we have, with the vacuum resin infusion process, performed the outer carbon and Kevlar layers, and after the final curing, glued with resin, a layer of 3m EasyCell75. After this glue has hardened, we have again, with the vacuum resin infusion process, performed the innermost carbon layer on top of the foam.

 

Unfortunately,the weight is almost the same, and it is apparently a weight gain that occurred during the infusion process in the foam, and the last carbon fiber layer. We know from the past that the carbon layer itself occupies only 50% resin by weight.

 

Why do we have this weight gain?

Wich methode should we use to reduce weight?

Is the infusion process and the foam not suitable?
Edited 8 Years Ago by Almand
Replies
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I think that when you vacuum infuse the inner skin the infusion process fills all of the foam cell surface with resin too and this is why it is heavy.

I have built around 100 3.3m sailing dinghy hulls that are basically 200g carbon, 4mm 100kg pvc foam and 200g carbon inside. In pre preg these hull shells typically weigh about 4.75kg and 9-10kg when finsihed with a deck and paint job. Once I tried an infused hull and it was 11kg so the infusion added 10% to the overall weight.

Your outer skin laminate of 200g carbon and 200g kevlar would be extremely strong. I would consider cutting the kevlar layer back to the lighter 80g kevlar instead.

I know that soric could be considered heavy with the flow channels full of resin but it works so well with infusion. Maybe try 1.5mm soric instead? With the lighter kevlar as mentioned. A round kayak hull shape will still have reasonable stiffness even with just 1.5 or 2mm soric.




Edited 8 Years Ago by Fasta
Almand
Almand
Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)
Group: Forum Members
Posts: 19, Visits: 108
Hi Fasta, thanks for reply

I think you are right about at least some of the foam cell er filled with resin, but i dont understand why, because the water uptake should be less than 1 %

How many sqm are the dinghy you make? I'm an old dinghy sailor (Laser, europe) so i´m a litte intersted in what type that is.

What kind of paint du you use, and do you paint in mould or after?

I think we will give soric lrc 1.5 a try, and a lighter kevlar layer. Combined with a better infusion control as mentioed in other posts, it could help us to reach our target. 

Best regards, Keld
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Almand (07/02/2017)
Hi Fasta, thanks for reply

I think you are right about at least some of the foam cell er filled with resin, but i dont understand why, because the water uptake should be less than 1 %

How many sqm are the dinghy you make? I'm an old dinghy sailor (Laser, europe) so i´m a litte intersted in what type that is.

What kind of paint du you use, and do you paint in mould or after?

I think we will give soric lrc 1.5 a try, and a lighter kevlar layer. Combined with a better infusion control as mentioed in other posts, it could help us to reach our target. 

Best regards, Keld


I build the hydrofoil moth class dinghies. Pre pregs and pvc foam but without any film glue that is often used for adhesion to cores. Panel weight is 1100g m2.
They come out with a lot of "weave porosity" which I fill will epoxy fillers, epoxy primers, automotive primers and then two part paint. 

The first filler is hard screeded to fill only the porosity, then epoxy primer. These two are then completely sanded off back to the carbon surface. Primed again with automotive primer, some spot fills and primer touch ups, wet sanded and painted the total paint jobs are less than 1kg but a lot of sanding work.

Hull shell surface area is about 3m2, with deck would be about 4m2.

Almand
Almand
Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)
Group: Forum Members
Posts: 19, Visits: 108
Wau - That´s a beautiful racing mashine, i would love to try it Smile
Best Regards Keld 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Almand - 8 Years Ago
MarkMK - 8 Years Ago
Almand - 8 Years Ago
FLD - 8 Years Ago
Almand - 8 Years Ago
Fasta - 8 Years Ago
Almand - 8 Years Ago
Fasta - 8 Years Ago
Almand - 8 Years Ago
oekmont - 8 Years Ago
Almand - 8 Years Ago
oekmont - 8 Years Ago
Almand - 8 Years Ago
Junior - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search