Hi all, I've just made a mould for a bootlid for an s1 exige using the uni-mould kit, I used 2k paint (colour) on the original lid and have noticed after releasing the mould that the 2k paint has gone soft and now shows print through from the coupling coat, is this normal?
I used Easylease on the surface (6 coats) followed by 2coats of wax to guarantee release. The 2k paint is 1month old and appeared to be solid before moulding.