Hi all,



I've got a few questions regarding the 'new' product 'XenCast Flexible Polyurethane Rubber' advertised on your website.

Basically I'm making a couple of moulds with the intention of casting 'Vac-Cast Epoxy Resin' into them,  what I need to end up with are two perfectly reproduced tooling plugs for vacuum forming my final parts into ABS plastic.



The following image will hopefully explain in greater detail my procedure.  I've recently used a product from 'Smooth-On' called 'OOMOO 30',  but had a disastrous result.  I must admit,  as good as it seems to be I just hate working with it.  Here's what my original mould box looks like with my plug secured in the base,  I then poured the silicon rubber into the mould box .........  it was an awful lot of work,  trying to mix what was a consistency of partly molten lava,  and the impossibility of pouring made the job needlessly difficult,  the result was a failed pour and a very badly formed mould  !  >>

 



Pouring the mix in a thin stream in a low corner was just impossible,  I almost had to resort to 'trowelling' it in ! >>

 



When I demoulded the following day,  it wasn't too bad,  but strictly speaking an appalling result.  Not something I would want to cast resin into that's for sure .........  I put it down to a good learning experience  >>





Because the silicon rubber wasn't 'fluid' enough,  full coverage of my plug wasn't achieved,  leaving large voids and air pockets  >>

 









So basically,  my question is,  would that 'XenCast flexible Polyurethane rubber'  be an alternative to OOMOO 30  ?

I've been looking at the 'XenCast PX30',  it seems to have the same characteristics as the OOMOO 30  ( both Shore A of 30 ),  how will it react to Vac-Cast Epoxy Resin being poured into it  ?







To further explain my situation my entire procedure is here >  Headlight mounting bracket moulds
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi Turk, Must have missed this one.

Although PX30 could be used in this way, as already pointed out, the PU lacks the self releasing properties you ideally would want.

CS25 seems a better all round solution having both the self releasing properties and also a much lower viscosity than the oomoo product you mentioned above.  The CS25 will pour into the mould boxes fairly easily  and being lower viscosity should be easy to mix too.  Like most silicones, if you are not degassing, we would recommend you stretch pour it to help remove any gas from mixing.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
TURK
TURK
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 101, Visits: 662
Hi Warren .......



No worries mate   Smile


I think I've just sent you an email ( EasyComposites - sales ) .........  With a barrage of questions,  sorry about that.  Looking at buying the Vacuum degassing system,  so a few questions in that department,  and a few questions about certain supplies that I couldn't find on the website,  but are listed in your brochure.

I've been talking to the company who supplied me the 'OOMOO 30' silicone rubber,  they have agreed that all is not well, and that it may be at fault .......  they're currently deciding whether they'll replace it FOC !  Satisfied

So,  I'm kind of stuck between a rock and a hard place right now.  I really wanted to order the CS25 at the same time as my degassing system,  shipping costs to France can be quite expensive !



Can I at this point ask about this 'Howto' that one of your colleagues made.  Very interesting stuff !  I know you've changed the vacuum pump from the one in the video as I've already asked that one,  but what silicon did your colleague use ?  >








Thanks









TURK







GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
nc42 - 9 Years Ago
TURK - 9 Years Ago
Rich (Staff) - 9 Years Ago
TURK - 9 Years Ago
Rich (Staff) - 9 Years Ago
TURK - 9 Years Ago
Rich (Staff) - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
Hanaldo - 9 Years Ago
Warren (Staff) - 9 Years Ago
TURK - 9 Years Ago
Warren (Staff) - 9 Years Ago
Rich (Staff) - 9 Years Ago
Hanaldo - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 9 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search