Group: Forum Members
Posts: 237,
Visits: 4.8K
|
I use 3M,other people swear by other polishes but I'm happy to pay the premium and use the fast cut an the fast cut plus.
once you master the 2002 its unlikely you will need to polish but in my application its for turbo pipes for a f1 engine and the spec/Finnish is very high.
we are using freecote 700,but only because its what the company uses I would much prefer mono coat !
in our application the part is made in pre preg and bag cooked.
once cured we de bag and put the part and mould in a oven at 140 and at this temp the printed part turns into a marshmallow consistency and is pulled from/out of the part.
item looks perfect as if it had come from a carbon mould
|