I'm vacuum-bagging a hand-layup using glass fibre fabric.
My mould is quite deep, so I overlapped two pieces of peel ply onto the wet fabric (which is also in two pieces).
But when I tried to remove the peel ply it had somehow stuck into the fabric and wouldn't come off.
Is it better to just use one single piece of peel ply and accept that it'll wrinkle?