Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Hand Layup
»
peel ply problem
peel ply problem
Post Reply
Like
3
peel ply problem
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
rocketeer
rocketeer
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 7
I'm vacuum-bagging a hand-layup using glass fibre fabric.
My mould is quite deep, so I overlapped two pieces of peel ply onto the wet fabric (which is also in two pieces).
But when I tried to remove the peel ply it had somehow stuck into the fabric and wouldn't come off.
Is it better to just use one single piece of peel ply and accept that it'll wrinkle?
Rick N
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
peel ply problem
rocketeer
-
9 Years Ago
There's no problem with peel ply wrinkling, as long as it doesn't bridge. The trouble with peel...
Hanaldo
-
9 Years Ago
[quote][b]Hanaldo (20/10/2016)[/b][hr]There's no problem with peel ply wrinkling, as long as it...
jdp530
-
8 Years Ago
Quick tip with the peel ply is to keep the red lines all running in the same direction, sounds...
VVS
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search