1960s fibreglass sidecar repair
1960s fibreglass sidecar repair
Post Reply
Like
6
1960s fibreglass sidecar repair
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Tincan3
Tincan3
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 12
Hello Folks,
I am hoping some of you kind people can save me a lot of time by advising on the best way & materials to repair the broken front of a 1960s sidecar body.
In my limited experience it is very difficult to get a good bond with old fibreglass using fresh polyester resin and glass fibre. There are so many new products available now such as carbon fibre or kevlar cloths and epoxy resins that I think there must be better material to use.
Many thanks for any suggestions.
Here is a photo of the damage (long story!).
Tags
old fibreglass repair
sidecar
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
1960s fibreglass sidecar repair
Tincan3
-
10 Years Ago
Yeh I'd use at least a vinyl ester, preferably an epoxy. Just have to scarf, clean and mechanically...
Hanaldo
-
10 Years Ago
Hanaldo, Many thanks. You suggest using an epoxy which I, too, was feeling would work better. Yes,...
Tincan3
-
10 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search