Hi Chris,
There can be a number of reasons, including bridging of the material or stack, bubbles in the resin etc, that can contribute to bubbles in the laminate - despite a perfectly sealed bag. It is hard to tell which is which without seeing where the bubbles are.
If you can post some pictures we will try to work out where things are going wrong.