Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Mould repairs
Mould repairs
Post Reply
Like
2
Mould repairs
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Chris Smith
Chris Smith
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 11,
Visits: 436
good morning all.
I have done a few moulds since my intro and I have just finished a mould and found it needs repairs doing in a small area. What would be the best way to repair any holes and cracks?
Thanks for your time and help in advance.
Reply
Like
2
Reply
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
If you watch EC's video of making a bonnet mould, they do a quick gelcoat repair in that video.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Mould repairs
Chris Smith
-
9 Years Ago
What kind of materials is the mould made from? Usually a gelcoat repair or even resin repair will...
scottracing
-
9 Years Ago
I am using tooling jel coat. That's what I thought but wanted to make sure first. Thanks
Chris Smith
-
9 Years Ago
If you watch EC's video of making a bonnet mould, they do a quick gelcoat repair in that video.
Hanaldo
-
9 Years Ago
Brill. I will sure take another look at it.
Chris Smith
-
9 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search