good morning all.
I have done a few moulds since my intro and I have just finished a mould and found it needs repairs doing in a small area. What would be the best way to repair any holes and cracks?
Thanks for your time and help in advance.
By Chris Smith
-
10/4/2016 6:38:07 PM
Brill. I will sure take another look at it.