ive been looking into composites for a while now and was under the impression that epoxy resins are the only resins that are used but just now I have come across the following

cyanite ester
bmi
polyimide

what can you tell me about these resins before I go spend hours researching on google

thanks,
Cole
Reply
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
If its the same as the prepreg version BMI is mad stuff ,its a ceramic prepreg

has n out life of about 10 minutes !

comes off the roll and the material is soaking wet almost like its wetlay

used it lots for heatshields in f1

throw in in a bag and cook at 180 an once its stripped its post cured to 450 if I remember correctly

very light parts an once post cured you can pick them up by hand straight out of the oven

you think you have cleaned your work area an tools down but next morning you will have a fine white powder on everything the material touched