ive been looking into composites for a while now and was under the impression that epoxy resins are the only resins that are used but just now I have come across the following

cyanite ester
bmi
polyimide

what can you tell me about these resins before I go spend hours researching on google

thanks,
Cole
By f1rob - 9/26/2016 9:56:17 PM

Total brain fade and too many materials !

one I just described isn't mbi !

used mbi on gearboxes,fairly normal to lay up but you have to double breather and release everything do to the resin dissolving bagging !!!