Hi. I've read elsewhere that a mould should typically be about 3 times the thickness of the part to be laid up in it.

Is this always the case or just moulds made using polyester resin? Would an epoxy/roving mould need to be so thick?

Dan
Reply
Dantheman
Dantheman
Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)
Group: Forum Members
Posts: 6, Visits: 116
Ah so the resin makes a difference...I was thinking of using regular epoxy (mainly to avoid the stink of poly/vinyl ester) and 600g roving in two lots of three layers?