Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
1 layer of 225 and then 4-5 layers of 450 is plenty if you're using tooling resin. That will give you a mould thickness of 5-6mm, which will be a very solid mould for most things. If you're using regular laminating resin without any fillers in it then you would probably want to do 6-8 layers of 450, and you would need to do it in 2 or 3 stages to prevent warping.
|