Thanks Davro !
in the 6th picture you can see where i sanded it down after its 2nd coat, Still some low spots but looked alright, the 7th picture where you can see all the low spots and what looks like gouges is after my father kinda let some water on it while 2hrs into a cure ha But the EL2 filled the low spots well and i was happy that i didn't need to scrap the part.
Looking forward to using the XCR, Should arrive Wednesday so i can start 1 item before i fly out for holidays on thursday ha
|