nope

a 1500mm x 650mm x 50mm sheet of epoxy block is roughly 3-400quid and the equivalent in ali would be a few grand at least.
Betamax
Betamax
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 3, Visits: 23
Isn't Aluminium cheaper than tooling board?
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Sire thing mate pm me or email direct

still busy getting the gt off the ground but still working towards my own stuff

just got a oven 4mt-3mt-3mt !

use to be used for indycar floors so should be big enough for anything I have to do !!!
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Well you know better than I do, but usually epoxy tooling block is good for between 6 -10 parts, you can use it more times but it depends on who's breaking the parts out and if you are cutting on the tool Smile

I've had a few small tooling block moulds made recently, and with the cost compared to an ali mould it would be cost effective on an A4 sized billet about 40-50mm thick  to have an ali tool made after 20 or so parts.

We need to chat too, got a few things on in the pipeline and I need to get setup properly.
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
To save me having to stress the grey matter has anyone got any figures on the breakdown where small/medium sized an fairly simple moulds cnc,d in Ali are cost affective over tooling block/carbon moulds

Rough mental arithmetic looks like 25plus parts would make the Ali more cost effective

Anyone ??????