Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
1.6m Wide hood skinning
1.6m Wide hood skinning
Post Reply
Like
3
1.6m Wide hood skinning
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
einar
einar
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 11
I like to skinning 1.6m wide hood, max carbon fiber that i can find is 1.5m wide, how is possible to connect two pieces of carbon fiber fabrics in center of hood.
Reply
Like
3
Reply
einar
einar
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 11
Hoods lenght is more than 1.5 m , is only one way "V weave" , is possible to find some video guide?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
1.6m Wide hood skinning
einar
-
8 Years Ago
It depends on the other dimension of the hood. Our maximum width cloth is, as you correctly say,...
Warren (Staff)
-
8 Years Ago
Hoods lenght is more than 1.5 m , is only one way "V weave" , is possible to find some video guide?
einar
-
8 Years Ago
We don't have a video guide ourselves for specifically V weave patterns. There may well be guides...
Warren (Staff)
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search