Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
polyester resin infusion
polyester resin infusion
Post Reply
Like
2
polyester resin infusion
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
magee
magee
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 25
hi guys just wandering is it possible to infuse polyester resin
Reply
Like
2
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
With an infusion grade polyester, absolutely.
Reply
Like
3
magee
magee
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 25
great any tip where to get it . i asked some suplyers they said i could use inhibitor to slow the curing time but i am woried it would boil in the wacuum
Reply
Like
2
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Easy Composites carry it:
https://www.easycomposites.co.uk/ip2-polyester-infusion-resin
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search