Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I assume you mean the 'marble' carbon fibre? Lamborghini use a pre-preg material for theirs. Someone over on Composites Central made a tutorial video for how to do it with wet lay, though it was a bit crude compared to the Lambo stuff though. I also can't see it working for skinning, you need a mould. Ita basically just a slurry of chopped up spread-tow fibres and resin.
|