Visits: 28K
|
Sounds like a thin coating. Looks outstanding, but if you want to find a coating that you don't have to spray in multiple coats, looks for high solids with good flow characteristics. Makes life so much easier, and you can generally fill the pinholes on the first wet coat by forcing it in with a brush, then it all levels out when you spray the second wet coat.
|