Hello all, 

I am currently doing some rearranging and making some upgrades to my work shop and one of my upgrades is to build a new table/work station that will be strictly used for composite work. I am currently in the design phase of this work station and would like to get some input from the experts on what type of material would be best to use as the final table top? 
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
A bench top covered with nylon sheet or similar is quite good. You can cut on it with knives and spilled resin or glue will not stick to it either.




SeftonMitchell
SeftonMitchell
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 5, Visits: 34
Awesome, thanks for the advice. I am going to price that tomorrow. I was originally going to using stainless steel but decided to find a more cost friendly option first lol. 
davro
davro
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
I use an old glass computer table for my composite workstation.
one side for mould making and the other side for flat sheet infusions with a fan heater underneath makes for a cheap low temp oven.

George Sychrovsky
George Sychrovsky
Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)
Group: Forum Members
Posts: 24, Visits: 1.6K
I put the white coated melamine on top of the bench, the white coating is a natural nonstick, I can still put screws into it to hold jigs and fixtures , with waxing the drips pop right off


---------------------------------------------------------------------
Disclaimer opinions of others will vary depending on what they are selling
Attachments
lgs06.JPG (339 views, 105.00 KB)
SeftonMitchell
SeftonMitchell
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 5, Visits: 34
That is a very good idea! I will definitely be considering this or at least incorporate it in my design one way or another! Thanks for the tip! Just got to find some used glass that will work. 
Edited 9 Years Ago by SeftonMitchell
Pugsport
Pugsport
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 14, Visits: 167
it might be worth checking the price of new glass as i bough a double glazed panel for my front room window for £40 and it was 1500x1500mm 
VVS
VVS
VVS
posted 9 Years Ago HOT
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
If you simply want a surface to work from then the choices are endless, if you want to produce flat sheet then a glass top is going to help.




if you in the UK Ikea sell very cheap glass table tops that can be adapted easily, when not needed you can simply use lining paper as a throw away cover, I got a few rolls and then tack them in place with some brown parcel tape.