moulding warping


Author
Message
FLD
FLD
FLD
posted 9 Years Ago HOT
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I went round to a friends house who's also a hobby moulder.  He's been having trouble with his mouldings warping.  They are CSM polyester and have moulded fine.  Over time (up to a year) they are warping really badly.  One example is a panel that has a 90 degree return / lip which has curled up beyond the 90 degree!  I've never had this and all I could come up with was demoulding too early.  Are there any other reasons he could be seeing this?
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Have you got photos? It does sound a little bit odd, but I've seen some serious distortion so it wouldn't surprise me. 
FLD
FLD
FLD
posted 9 Years Ago HOT
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
He won't let me take pics, he's too embarrassed!  I wonder if it's different catalyst levels in gelcoat to laminate or gelcoat not cured enough when he layed up onto it. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...