moulding warping


Author
Message
FLD
FLD
FLD
posted 9 Years Ago HOT
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I went round to a friends house who's also a hobby moulder.  He's been having trouble with his mouldings warping.  They are CSM polyester and have moulded fine.  Over time (up to a year) they are warping really badly.  One example is a panel that has a 90 degree return / lip which has curled up beyond the 90 degree!  I've never had this and all I could come up with was demoulding too early.  Are there any other reasons he could be seeing this?
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It's just shrinkage. Polyester shrinks horrendously, and does so for a long time. Unbalanced laminates make it much worse, and csm distorts easily because it is short strands. The natural modulus of a part will also play a role, flat sheets distort easier than a part with curvature. 