Evening Chaps,



I have a technical question that I can't seem to work out what is causing my problem on carbon piece I'm making at the moment.

The part I'm making is a shroud protector for hovercraft fan. Its made up of 8 identical parts the will have joiners in-between to make a full circle when finished. So the part is a 1/8 of a circle arch that is hollow tube.

I have my mould and I'm using pre preg carbon with a bladder insert as the shape is cylindrical and hollow.

Currently curing at 25Degrees for 8hours and with the bladder at around 14psi.

The problem I'm getting after pulling the part is that is doesn't natural go back into the mould and rest. Seems to have flexed or pulled in or shrunk I'm not to sure for the technical term for it.

So my question what can cause this, i wonder if when curing my mould could have moved with the heat. But I can't seem to work out what might have caused this issue. 

I have attached some photos that can hopefully better show you what I'm describing.

Regards

Chris
Attachments
IMG_6510.JPG (289 views, 1.00 MB)
IMG_6511.JPG (298 views, 2.00 MB)
IMG_6506.JPG (283 views, 1.00 MB)
Reply
RTM
RTM
RTM
posted 9 Years Ago HOT
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 34
Thanks for the reply,

Yes part is given plenty of time to get back to ambient temperature and then left over night.

For layup i'm just using 1 long piece throughout the mould on both top and bottom sections.

Do you think there would be a better layup to prevent the part from bending out of place?