RTM
RTM
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 34
Evening Chaps,
I have a technical question that I can't seem to work out what is causing my problem on carbon piece I'm making at the moment.
The part I'm making is a shroud protector for hovercraft fan. Its made up of 8 identical parts the will have joiners in-between to make a full circle when finished. So the part is a 1/8 of a circle arch that is hollow tube.
I have my mould and I'm using pre preg carbon with a bladder insert as the shape is cylindrical and hollow.
Currently curing at 25Degrees for 8hours and with the bladder at around 14psi.
The problem I'm getting after pulling the part is that is doesn't natural go back into the mould and rest. Seems to have flexed or pulled in or shrunk I'm not to sure for the technical term for it.
So my question what can cause this, i wonder if when curing my mould could have moved with the heat. But I can't seem to work out what might have caused this issue.
I have attached some photos that can hopefully better show you what I'm describing.
Regards
Chris
Attachments
IMG_6510.JPG
(
290 views,
1.00 MB
)
IMG_6511.JPG
(
299 views,
2.00 MB
)
IMG_6506.JPG
(
284 views,
1.00 MB
)
Reply
Like
3
Reply
scottracing
scottracing
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
If you are only using a single ply it will be difficult to counteract the spring action without adding more material.
Are you using a twill fabric or ud?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Tech question for srinkage on carbon part
RTM
-
9 Years Ago
curved components will always move about depending on your layup, have you gone quasi layup in your...
scottracing
-
9 Years Ago
Thanks for the reply, Yes part is given plenty of time to get back to ambient temperature and then...
RTM
-
9 Years Ago
If you are only using a single ply it will be difficult to counteract the spring action without...
scottracing
-
9 Years Ago
Just the EC pre pre twill at the moment, but if there is a better material or number of layers or...
RTM
-
9 Years Ago
14 psi is not much pressure but the bladder process does rely completely on the stiffness of the...
Fasta
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search