Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
what material would work best
what material would work best
Post Reply
Like
3
what material would work best
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
vmax1974
vmax1974
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 98
I have been asked bu a customer to make a fibreglass shelf for a gridwall display
now since its a one off I was thinking about using pieces of perspex to make a makeshift mould now I am using polyester resin and gel so I want to know will the perspex react to the gel and will it release ok with a good finish on the part
Will it work or has anyone got any better ideas
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
what material would work best
vmax1974
-
9 Years Ago
You could try the perspex and polyester resin, it would be a good learning experience... But...
ChrisR
-
9 Years Ago
Local glass suppliers it is then thanks
vmax1974
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search