Hi, new here.

Only done a couple of simple carbon parts before but have a slightly more ambitious project in mind which I don't know how best to approach. How would you set about making a fairly thick section solid carbon part - think something like HANS device (don't worry I'm not attempting to make my own HANS!).

I understand the principles of vacuum bagging but if you have a split enclosed mould (like an injection mould tool), how would you ensure complete fill, create the pressure and where would you evacuate any excess resin (assuming pre-preg)?

I guess the tool would want to be aluminium and heated so as not to take too long to come up to temp in an oven?

Thanks for your assistance.
Edited 9 Years Ago by crice
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
@ fgayford ..

I'll try to dig out the few photos I have of the process .. the mould now resides on another island, and even if my country is small, its still a bit of a drive to get there (across 3 bridges, one of which is the worlds 2. longest suspension bridge .. )
I'll try to get my friend to email me a few photos ...

I do have a few much simpler alu moulds, that work the same way .. I'll dig them out and do a test run .. with a few pictures along the way --

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 9 Years Ago by Dravis
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search