I have a mould for a 7 type nosecone that has had its day so I need to make a new mould 

I have been pulling parts from it hoping that I may be able fettle and gelcoat repair one but the front edge of the mould is in poor shape 

http://www.talkcomposites.com/Uploads/Images/2db2b604-abcf-4720-b583-b090.jpg


this is what pulls from the mould Most of the part pulls with a nice finish

i have been looking at the patten coatings so my question is should i sand and getcoat filler the edge and flog that horse or sand fill then spray pattern coat 