67redrocket
67redrocket
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I have heard that bondo dont stick to epoxy primer.
What about epoxy resin? I have a part that I have made with epoxy resin, can I use bondo on it and then paint it?
Reply
Like
7
Reply
f1rob
f1rob
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
What car is it for ???
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bondo on epoxy?
67redrocket
-
9 Years Ago
I've never had any issues.
Hanaldo
-
9 Years Ago
I keep hearing references to this "Bondo" -- What is that exactly? Some kind of Polyester...
Dravis
-
9 Years Ago
Bondo is just a brand (the original brand I believe) of polyester body filler.
Hanaldo
-
9 Years Ago
[quote][b]Hanaldo (31/03/2016)[/b][hr]Bondo is just a brand (the original brand I believe) of...
67redrocket
-
9 Years Ago
A polyester will stick to an epoxy a lot better than a epoxy will stick to a polyester even thou the...
f1rob
-
9 Years Ago
[quote][b]f1rob (31/03/2016)[/b][hr]A polyester will stick to an epoxy a lot better than a epoxy...
Hanaldo
-
9 Years Ago
[quote][b]Hanaldo (05/04/2016)[/b][hr][quote][b]f1rob (31/03/2016)[/b][hr]A polyester will stick to...
fgayford
-
9 Years Ago
youll be fine. Ive often had to fix little spots after I have sanded the primer and the guide coat...
kidpaint
-
9 Years Ago
When I first got into this game 82/83 ish pre preg had only been out (or I should say in use in f1)...
f1rob
-
9 Years Ago
If they were with Lotus then I don't believe a word they said, their panels are the worst I've...
Hanaldo
-
9 Years Ago
One of my proud boasts is to say I have never worked for lotus cars ! some of the bodies done with...
f1rob
-
9 Years Ago
The Lotus stuff I've worked with I would swear they haven't used any moulds. Or any form of...
Hanaldo
-
9 Years Ago
What car is it for ???
f1rob
-
9 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search