Bondo on epoxy?
Bondo on epoxy?
Post Reply
Like
7
Bondo on epoxy?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I have heard that bondo dont stick to epoxy primer.
What about epoxy resin? I have a part that I have made with epoxy resin, can I use bondo on it and then paint it?
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bondo on epoxy?
67redrocket
-
10 Years Ago
I've never had any issues.
Hanaldo
-
10 Years Ago
I keep hearing references to this "Bondo" -- What is that exactly? Some kind of Polyester...
Dravis
-
10 Years Ago
Bondo is just a brand (the original brand I believe) of polyester body filler.
Hanaldo
-
10 Years Ago
[quote][b]Hanaldo (31/03/2016)[/b][hr]Bondo is just a brand (the original brand I believe) of...
67redrocket
-
10 Years Ago
A polyester will stick to an epoxy a lot better than a epoxy will stick to a polyester even thou the...
f1rob
-
10 Years Ago
[quote][b]f1rob (31/03/2016)[/b][hr]A polyester will stick to an epoxy a lot better than a epoxy...
Hanaldo
-
10 Years Ago
[quote][b]Hanaldo (05/04/2016)[/b][hr][quote][b]f1rob (31/03/2016)[/b][hr]A polyester will stick to...
fgayford
-
10 Years Ago
youll be fine. Ive often had to fix little spots after I have sanded the primer and the guide coat...
kidpaint
-
10 Years Ago
When I first got into this game 82/83 ish pre preg had only been out (or I should say in use in f1)...
f1rob
-
10 Years Ago
If they were with Lotus then I don't believe a word they said, their panels are the worst I've...
Hanaldo
-
10 Years Ago
One of my proud boasts is to say I have never worked for lotus cars ! some of the bodies done with...
f1rob
-
10 Years Ago
The Lotus stuff I've worked with I would swear they haven't used any moulds. Or any form of...
Hanaldo
-
10 Years Ago
What car is it for ???
f1rob
-
10 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search