Bondo on epoxy?


Author
Message
67redrocket
67redrocket
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 49, Visits: 486
I have heard that bondo dont stick to epoxy primer. 

What about epoxy resin? I have a part that I have made with epoxy resin, can I use bondo on it and then paint it?
Reply
kidpaint
kidpaint
Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)
Group: Forum Members
Posts: 99, Visits: 676
youll be fine. Ive often had to fix little spots after I have sanded the primer and the guide coat showed the low spot. Make sure the primer is rough sanded so it has a bite for the filler to stick to
Edited 9 Years Ago by kidpaint
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
67redrocket - 9 Years Ago
Hanaldo - 9 Years Ago
Dravis - 9 Years Ago
Hanaldo - 9 Years Ago
67redrocket - 9 Years Ago
f1rob - 9 Years Ago
Hanaldo - 9 Years Ago
fgayford - 9 Years Ago
kidpaint - 9 Years Ago
f1rob - 9 Years Ago
Hanaldo - 9 Years Ago
f1rob - 9 Years Ago
Hanaldo - 9 Years Ago
f1rob - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search