Bondo on epoxy?


Author
Message
67redrocket
67redrocket
Supreme Being (413 reputation)Supreme Being (413 reputation)Supreme Being (413 reputation)Supreme Being (413 reputation)Supreme Being (413 reputation)Supreme Being (413 reputation)Supreme Being (413 reputation)Supreme Being (413 reputation)Supreme Being (413 reputation)
Group: Forum Members
Posts: 49, Visits: 486
I have heard that bondo dont stick to epoxy primer. 

What about epoxy resin? I have a part that I have made with epoxy resin, can I use bondo on it and then paint it?
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I keep hearing references to this "Bondo" -- What is that exactly?   Some kind of Polyester filler/primer?

I use cheap polyester filler on a lot of my patterns, I've never had any problems with mixing it with Epoxy .. As long as it is allowed to cure for at least 24 hours .

I often make patterns out of cheap floor insulation foam .. it will "melt" when in contact with the EC pattern primer, so I "seal it" with a layer of epoxy, leave it to cure for 24 hours, key it with 120 grit, then use polyester filler and EC pattern Coat primer -  If I accidentally sand all the way through to the foam, I just re-seal it with epoxy, then carry on with the Pattern Coat primer ..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 9 Years Ago by Dravis
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
67redrocket - 9 Years Ago
Hanaldo - 9 Years Ago
Dravis - 9 Years Ago
Hanaldo - 9 Years Ago
67redrocket - 9 Years Ago
f1rob - 9 Years Ago
Hanaldo - 9 Years Ago
fgayford - 9 Years Ago
kidpaint - 9 Years Ago
f1rob - 9 Years Ago
Hanaldo - 9 Years Ago
f1rob - 9 Years Ago
Hanaldo - 9 Years Ago
f1rob - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search