Sorry yet another question I do try and look up the answer on the net before asking 

But the front wings on a car are the moulds done in one or 2 piece 

I thought where they bolt inside the engine bay would have to be done separate but might be wrong?

http://www.talkcomposites.com/Uploads/Images/c2b02bc9-e808-43d4-a786-d495.jpg


http://www.talkcomposites.com/Uploads/Images/31bd8f4c-6256-437f-b863-3e27.jpg
http://www.talkcomposites.com/Uploads/Images/e6d35f89-575e-4d7e-b015-b284.jpg
http://www.talkcomposites.com/Uploads/Images/934f11ad-5b7d-4c0c-9381-bd4d.jpg
kidpaint
kidpaint
Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)
Group: Forum Members
Posts: 99, Visits: 676
I may be wrong but I believe that part is made in 1 piece, but the part where it goes behind by the door I think it too much of an angle to make it out of 1 piece. Maybe yours doesnt do that, its hard to tell from the pics
Edited 9 Years Ago by kidpaint
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
Yea the part that goes behind the is tight is that part needed though as it doesn't bolt there 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Is there nothing securing the fender to the front bumper or headlight? Lip around the inside of the wheel arch? Those 2 areas would give you a lock for sure. 

I would be making this a split mould on the top edge of the guard, so as you said about the mounting surface in the engine bay. Doing it like this not only guarantees that you will get a release, but it also makes the entire flanging job a bit less tricky. You may be able to do it in one piece, but you would need to put more thought into how you flange it. 
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
I'll get a couple more pic's of the said mounting points 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search