Wheel arch liners for my little plastic skip are getting scarce and are freekin' dear from GM/vxl.  Some of the owners have considered making them and the flexible resin often crops up.  Not best for the job IMO.  Anyone ever made arch liners with any success?  The OEM plastic is nice and tough 600 quid each is a bit OTT though.
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
FLD (28/03/2016)
Perfect, what resin did you use?


Infused with Araldite LY3600. Pretty standard laminating epoxy. Didn't have to use flexible resin, the sheet thickness is only about 1mm so it's flexible enough. 

Flexible resin wouldn't hurt though, I just don't have access to any here. 