Hi Lasse,
you can grind back a little then add some more tooling gel ( remember to release coat the other faces) and then sand back.
you could cover the repair and it will cure ok or add some solution wax to give a dry surface.
don't go mad trying to get perfect joins, you need to seal the flanges with silicon and this does a good job of filling small voids, use the automotive type but if you are using easy lease go careful at these joins as it slightly dissolves the silicon.
|