Unimould repair?


Author
Message
svedberg
svedberg
Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)
Group: Forum Members
Posts: 22, Visits: 173
I have a 6-piece mould made from the Unimould system. There are a few minor imperfections along the parting lines that needs to be adressed before using the mould.

Can I build up  the (very small) broken off edges using the Unimould tooling gelcoat? Any special measures to be taken (wax mixing into the gelcoat)?

Thanks in advance!

Lasse Svedberg

Racing motorcycles!
Reply
svedberg
svedberg
Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)Supreme Being (180 reputation)
Group: Forum Members
Posts: 22, Visits: 173
Yes, I'll envelope bag the whole thing. My issue is these small broken off pieces along the mould parting lines...but I guess I'll use some Unimould tooling gelcoat to fix these. What exactly is the kind of "wax" to be mixed into the gelcoat, and at which rate?

Thanks/

Lasse

Racing motorcycles!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search