Which resin for large, crystal clear, UV resistant casting?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Woodie
Woodie
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 8
I have a project that requires making relatively large castings (up to 1 litre in a single pour) of crystal clear epoxy that is both UV stable and can be polished to a high gloss finish.
Any recommendations on suitable resins (and any tips) greatly appreciated.
Phil
Reply
Like
18
Fasta
Fasta
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Epoxy resins are not known for their UV stability.
What about a polyurethane resin??
Fastacraft Facebook page
Reply
Like
19
Woodie
Woodie
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 8
Thanks Fasta, sorry for the late reply - my wife took both our laptops interstate!!
My main concern with poly is temperature & moisture. I live in a cool/humid area. Keeping my workshop above 20 centigrade for 3 days while the resin cures will be a pain in winter & storage also presents as a problem over the colder months.
Hence my leaning toward epoxy
Cheers
Phil
Reply
Like
18
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
You would need to keep the epoxy relatively warm too. 20 degrees is ideal, and I don't work if it's colder than 15.
Is local heating out of the question? A set of 500w work lights create a lot of heat, or a box and a small heater. I agree with Fasta, epoxy wouldn't be my first choice given your requirements.
Reply
Like
17
Fasta
Fasta
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
A 1kg part is not so big, could you take it into your home for a few days while it cures?
All these resin systems will require around 20-25C for curing , epoxies or polyurethane.
Fastacraft Facebook page
Reply
Like
16
Woodie
Woodie
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 8
Certainly sounds like Poly is the way to go. My workshop is solar powered hence my hesitance re heating for long periods - a light bulb based heating box is a great idea. Like it 😀. Many thanks for all the feedback.
Reply
Like
19
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
18
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search