Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Resin Casting and Moulding Forum
»
Clear Casting and Coating
»
Which resin for large, crystal clear, UV resistant casting?
Which resin for large, crystal clear, UV resistant casting?
Post Reply
Like
18
Which resin for large, crystal clear, UV resistant casting?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Woodie
Woodie
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 8
I have a project that requires making relatively large castings (up to 1 litre in a single pour) of crystal clear epoxy that is both UV stable and can be polished to a high gloss finish.
Any recommendations on suitable resins (and any tips) greatly appreciated.
Phil
Reply
Like
18
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Which resin for large, crystal clear, UV resistant casting?
Woodie
-
10 Years Ago
Epoxy resins are not known for their UV stability. What about a polyurethane resin??
Fasta
-
10 Years Ago
Thanks Fasta, sorry for the late reply - my wife took both our laptops interstate!! My main concern...
Woodie
-
10 Years Ago
You would need to keep the epoxy relatively warm too. 20 degrees is ideal, and I don't work if it's...
Hanaldo
-
10 Years Ago
A 1kg part is not so big, could you take it into your home for a few days while it cures? All...
Fasta
-
10 Years Ago
Certainly sounds like Poly is the way to go. My workshop is solar powered hence my hesitance re...
Woodie
-
10 Years Ago
Post Reply
Like
18
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search